Modulus of Elasticity 0.225 - 3.95 GPa
32.6 - 573 ksi
Average value: 2.28 GPa Grade Count:28
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 0.225 - 7.80 GPa
32.6 - 1130 ksi
Average value: 2.37 GPa Grade Count:101
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..