Mechanical Properties Metric English Comments
Modulus of Elasticity 4.30 - 10.0 GPa
624 - 1450 ksi
Average value: 6.97 GPa Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Modulus of Elasticity 4.30 GPa
624 ksi
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Modulus of Elasticity 4.30 GPa
624 ksi
ISO 527-1/-2
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned)
Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles..
Modulus of Elasticity 4.30 GPa
624 ksi
Murtfeldt Murpec® Polyetheretherketone
In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change..
Modulus of Elasticity 4.30 - 7.80 GPa

@Temperature 60.0 - 120 °C
624 - 1130 ksi

@Temperature 140 - 248 °F
Average value: 6.02 GPa Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Modulus of Elasticity 4.30 GPa
624 ksi
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts..
Modulus of Elasticity 4.30 - 11.5 GPa

@Temperature 60.0 - 175 °C
624 - 1670 ksi

@Temperature 140 - 347 °F
Average value: 6.88 GPa Grade Count:10
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..