Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 120 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 100A CP Titanium
Industry Specifications: USA Aerospace: AMS 4921. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specifications BS TA. 7, 8, 9.Features: The mechanical prope..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: ..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries ..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5),
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are ..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET 75A CP Titanium (ASTM Grade 4)
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET CP Titanium (ASTM Grade 3)
Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA
Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy
Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET.
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2)
Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical; Solution treated
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy;
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed;
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed;
Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A ..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® Code 12 Titanium Alloy (ASTM Grade 12)
Features: Highly weldable, near-alpha alloy, exhibiting improved strength and temperature capability over CP combined with superior crevice corrosion resistance and excellent resistance under oxidiz..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed
Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w..
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy
Medium-Strength Surgical Implant AlloyFeatures: TIMETAL 367 is a dedicated, medium strength, titanium alloy for surgical implants. The alloy was developed specifically for the manufacture of femora..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Copyright © lookpolymers.com All Rights Reserved