Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2)

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer TIMET
Trade Name TIMETAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3, 4, 5.Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 50A is equivalent to ASTM Grade 2. It is the "workhorse" for industrial applications, having a guaranteed minimum 0.2% yield strength and good ductility and formability. It is used extensively for sea water piping, reactor vessels and heat exchangers throughout the CPI, Petrochemical, Oil and Gas and Naval/Marine markets. This alloy is also ASME approved, has good impact properties at low temperatures, and has excellent resistance to erosion and corrosion by seawater and marine atmospheres. It can be easily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 485 MPa
70300 psi
Typical
Tensile Strength, Yield 345 MPa

@Strain 0.200 %
50000 psi

@Strain 0.200 %
Typical
Elongation at Break 28 %
28 %
Typical
Reduction of Area 57 %
57 %
Typical
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
Fatigue Strength 154 MPa

@# of Cycles 1.00e+7
22300 psi

@# of Cycles 1.00e+7
Notched, Kt=3; rotating bend
232 MPa

@# of Cycles 1.00e+7
33600 psi

@# of Cycles 1.00e+7
Smooth, Kt=1; rotating bend
Bend Radius, Minimum 2.5 t
2.5 t
Typical; on 0.078 in (2 mm) sheet
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C

@Temperature 20.0 - 100 °C
4.78 µin/in-°F

@Temperature 68.0 - 212 °F
9.50 µm/m-°C

@Temperature 20.0 - 300 °C
5.28 µin/in-°F

@Temperature 68.0 - 572 °F
9.70 µm/m-°C

@Temperature 20.0 - 500 °C
5.39 µin/in-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 21.79 W/m-K
151.2 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C
797 °F
Continuous
540 °C
1000 °F
Intermittent
Beta Transus 915 °C
1680 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti >= 98.9 %
>= 98.9 %
Calculated as remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000530 ohm-cm
0.0000530 ohm-cm
Copyright © lookpolymers.com All Rights Reserved