Mechanical Properties Metric English Comments
Modulus of Elasticity 110 GPa
16000 ksi
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal
Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals.
Modulus of Elasticity 110 GPa
16000 ksi
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal
Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals.
Modulus of Elasticity 110 GPa
16000 ksi
PCC-Advanced Forming Technology 30% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Modulus of Elasticity 110 GPa
16000 ksi
Schott N-LAF36 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical; Solution treated
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy;
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Modulus of Elasticity 110 GPa
16000 ksi
Wieland Porta Maximum NF PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Modulus of Elasticity 110 - 120 GPa
16000 - 17400 ksi
Typical
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Modulus of Elasticity 110 GPa
16000 ksi
Tension
ECOMold 135 Copper Mold Material
ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T..
Modulus of Elasticity 110 GPa
16000 ksi
Bar, Rod & Forgings
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..
Modulus of Elasticity 110 GPa
16000 ksi
Castings & Strip
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..
Modulus of Elasticity 110 GPa
16000 ksi
Alliance S-20A Samarium Cobalt Magnetic Material
Modulus of Elasticity 110 GPa
16000 ksi
Alliance S-20B Samarium Cobalt Magnetic Material
Modulus of Elasticity 110 GPa

@Temperature 1200 °C
16000 ksi

@Temperature 2190 °F
ATI Wah Chang Nb/Nb Alloy FS-85
Information provided by ATI Wah Chang
Modulus of Elasticity 110 GPa
16000 ksi