Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Near Alpha Titanium Alloy
Manufacturer TIMET
Trade Name TIMETAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure vessels and piping also utilize this alloy. Available with palladium stabilization to enhance corrosion resistance. The alloy is cold formable and easily welded, such like the commercially pure grades of titanium. Yet the alloys offer nearly double the strength over TIMETAL 50A. It is ASME Boiler and Pressure Vessel code approved. It offers the highest structural efficiency of any of the common engineering metals approved by ASME. The alloy is available in all common product forms including billet, bar, plate, sheet, strip, tubing and pipe. It is nonmagnetic.Typical heat treatment for this alloy: Stress Relief: 316-649°C for .5-3 hrs, air cool. Anneal: 649-760°C for 1-3 hrs, air cool. Solution treat: 871-927°C for .25-1 hrs, water quench. Aging: 482-538°C for 2-8 hrs, air cool.Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 862 MPa
>= 125000 psi
Tensile Strength, Yield >= 724 MPa
>= 105000 psi
Elongation at Break >= 10 %
>= 10 %
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
Poissons Ratio 0.30
0.30
Shear Modulus 43.0 - 45.0 GPa
6240 - 6530 ksi
Thermal Properties Metric English Comments
CTE, linear 9.61 µm/m-°C

@Temperature 20.0 - 95.0 °C
5.34 µin/in-°F

@Temperature 68.0 - 203 °F
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
Melting Point <= 1700 °C
<= 3090 °F
Liquidus 1700 °C
3090 °F
Beta Transus 935 °C
1720 °F
Component Elements Properties Metric English Comments
Aluminum, Al 2.5 - 3.5 %
2.5 - 3.5 %
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.25 %
<= 0.25 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.15 %
<= 0.15 %
Titanium, Ti 92.6 - 95.5 %
92.6 - 95.5 %
Calculated as remainder
Vanadium, V 2.0 - 3.0 %
2.0 - 3.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000127 ohm-cm
0.000127 ohm-cm