Material Notes:
BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 1603.
Physical Properties Metric English Comments
Specific Gravity 1.95 - 2.01 g/cc
1.95 - 2.01 g/cc
Water Absorption 0.17 - 0.23 %
0.17 - 0.23 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
Tensile Strength, Ultimate 37.9 - 44.8 MPa
5500 - 6500 psi
Flexural Strength 82.7 - 89.6 MPa
12000 - 13000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 193 - 207 MPa
28000 - 30000 psi
Izod Impact, Notched 2.14 - 2.67 J/cm
4.00 - 5.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 17.2 kV/mm
436 kV/in
Short Time
Dissipation Factor 0.015

@Frequency 60 Hz
0.015

@Frequency 60 Hz
Condition A
0.027

@Frequency 60 Hz
0.027

@Frequency 60 Hz
Condition D
0.099

@Frequency 60 Hz
0.099

@Frequency 60 Hz
Condition A
0.124

@Frequency 60 Hz
0.124

@Frequency 60 Hz
Condition D
Arc Resistance 182 sec
182 sec
Track Resistance 8.33 sec
8.33 sec
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F