Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 193 - 228 MPa | 28000 - 33000 psi | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Compressive Strength | 193 - 228 MPa | 28000 - 33000 psi | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |