Polymer Property : Compressive Strength = 33000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 193 - 228 MPa
28000 - 33000 psi
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester
BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
Compressive Strength 193 - 228 MPa
28000 - 33000 psi
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit..