Material Notes:
Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Water Absorption 0.12 %
0.12 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 97.0 MPa
14100 psi
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 6.30 J/cm
11.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 10.2 kV/mm
259 kV/in
ASTM D149