Mechanical Properties Metric English Comments
Tensile Strength 28.0 MPa
4060 psi
ISO 527
Murtfeldt Muralen® Polyethylene
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Tensile Strength 28.0 MPa
4060 psi
at Yield; ISO 527-1/-2
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..
Tensile Strength 28.0 MPa
4060 psi
DIN 53288
Permabond TA4310 Toughened Acrylic Adhesive
PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
Tensile Strength 28.0 MPa
4060 psi
Indium Corp. Sn992 Pb-Free Soldering Alloy
Sn992 Pb-Free solder is a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross (in..
Tensile Strength 28.0 MPa
4060 psi
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy
Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn..
Tensile Strength 28.0 MPa
4060 psi
ASTM D412
GRECO ISOTHANE 1180A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength 28.0 MPa
4060 psi
ASTM D412
GRECO ISOTHANE 1185A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength 28.0 MPa
4060 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1153 A (SBS) Liner Block Copolymer
Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Tensile Strength 28.0 MPa
4060 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1153 E (SBS) Liner Block Copolymer
Description: Kraton D1153 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Kraton® D1155 E (SBS) Liner Block Copolymer
Description: Kraton D1155 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Europe in the physical form identified: Kraton D1155..
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Kraton® D1155 J (SBS) Liner Block Copolymer
Description: Kraton D1155 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Japan in the physical form(s) outlined in the grade..
Tensile Strength 28.0 MPa
4060 psi
Measured on films cast from a toluene solution; ISO 37
Kraton® D1161 B (SIS) Linear Block Copolymer
Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra..
Tensile Strength 28.0 MPa
4060 psi
Measured on films cast from a toluene solution; ISO 37
Kraton® D1161 E (SIS) Linear Triblock Copolymer
Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 E..
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Kraton® D1161 J (SIS) Linear Triblock Copolymer
Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t..
Tensile Strength 28.0 MPa
4060 psi
DIN 53455
Isoflon PEHD 500 High Density Polyethylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Tensile Strength 28.0 - 40.0 MPa
4060 - 5800 psi
DIN 53455
Isoflon TFM
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 28.0 MPa
4060 psi
100 micron film; ASTM D882
Kaneka PHBH Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Tensile Strength 28.0 MPa
4060 psi
ISO 527
MRC Polymers MAXTELâ„¢ 650-BK Polypropylene Homopolymer
• For injection molding• Excellent process ability with high flow.Information provided by MRC Polymers Inc.
Tensile Strength >= 28.0 MPa
>= 4060 psi
Excellent
Shandong Dongyue Polymer DF-203 PTFE Fine Powder
Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside...
Tensile Strength >= 28.0 MPa
>= 4060 psi
Excellent
Shandong Dongyue Polymer DF-204 PTFE Fine Powder
Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s..
Tensile Strength >= 28.0 MPa
>= 4060 psi
Excellent
Shandong Dongyue Polymer DF-205 PTFE Fine Powder
Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba..
Tensile Strength 28.0 MPa
4060 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 28.0 MPa
4060 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 28.0 MPa
4060 psi
ASTM D638
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Tensile Strength 28.0 MPa
4060 psi
ISO 527
Ecomass® 1080ZC86 Stainless Steel Powder Filled Polyamide Alloy, Injection Molding
Stainless Steel Powder Filled Polyamide Alloy, Very Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shield..
Tensile Strength 28.0 MPa

@Strain 300 %
4060 psi

@Strain 300 %
ISO 37
BASF Elastollan 1198 A TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Tensile Strength 28.0 MPa

@Strain 5.00 %,
Temperature 40.0 °C
4060 psi

@Strain 5.00 %,
Temperature 104 °F
50 mm/min; ISO 527-2
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 28.0 MPa
4060 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 28.0 - 36.0 MPa
4060 - 5220 psi
DIN 53455
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Copyright © lookpolymers.com All Rights Reserved