Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 28.0 MPa | 4060 psi | ISO 527 |
Murtfeldt Muralen® Polyethylene Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | DIN 53288 |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Tensile Strength | 28.0 MPa | 4060 psi | |
Indium Corp. Sn992 Pb-Free Soldering Alloy Sn992 Pb-Free solder is a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross (in.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | |
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D412 |
GRECO ISOTHANE 1180A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D412 |
GRECO ISOTHANE 1185A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1153 A (SBS) Liner Block Copolymer Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1153 E (SBS) Liner Block Copolymer Description: Kraton D1153 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ISO 37 |
Kraton® D1155 E (SBS) Liner Block Copolymer Description: Kraton D1155 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Europe in the physical form identified: Kraton D1155.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ISO 37 |
Kraton® D1155 J (SBS) Liner Block Copolymer Description: Kraton D1155 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Japan in the physical form(s) outlined in the grade.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | Measured on films cast from a toluene solution; ISO 37 |
Kraton® D1161 B (SIS) Linear Block Copolymer Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | Measured on films cast from a toluene solution; ISO 37 |
Kraton® D1161 E (SIS) Linear Triblock Copolymer Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 E.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ISO 37 |
Kraton® D1161 J (SIS) Linear Triblock Copolymer Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | DIN 53455 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Strength | 28.0 - 40.0 MPa | 4060 - 5800 psi | DIN 53455 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | 100 micron film; ASTM D882 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ISO 527 |
MRC Polymers MAXTEL™ 650-BK Polypropylene Homopolymer • For injection molding• Excellent process ability with high flow.Information provided by MRC Polymers Inc. |
|||
Tensile Strength | >= 28.0 MPa | >= 4060 psi | Excellent |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Tensile Strength | >= 28.0 MPa | >= 4060 psi | Excellent |
Shandong Dongyue Polymer DF-204 PTFE Fine Powder Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s.. |
|||
Tensile Strength | >= 28.0 MPa | >= 4060 psi | Excellent |
Shandong Dongyue Polymer DF-205 PTFE Fine Powder Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D638 |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ISO 527 |
Ecomass® 1080ZC86 Stainless Steel Powder Filled Polyamide Alloy, Injection Molding Stainless Steel Powder Filled Polyamide Alloy, Very Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shield.. |
|||
Tensile Strength | 28.0 MPa @Strain 300 % |
4060 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 28.0 MPa @Strain 5.00 %, Temperature 40.0 °C |
4060 psi @Strain 5.00 %, Temperature 104 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 28.0 MPa | 4060 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1290 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 28.0 - 36.0 MPa | 4060 - 5220 psi | DIN 53455 |
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |