Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 20.0 - 40.0 MPa
2900 - 5800 psi
Compression; ISO 527
Raschig Group DECAL® 937 Phenolic
Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W..
Tensile Strength 25.0 - 40.0 MPa
3630 - 5800 psi
Compression; ISO 527
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Tensile Strength 28.0 - 40.0 MPa
4060 - 5800 psi
DIN 53455
Isoflon TFM
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 32.0 - 40.0 MPa
4640 - 5800 psi
DIN 53455
Isoflon PCTFE Polychlorotrifluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 30.0 - 40.0 MPa
4350 - 5800 psi
ISO 527
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound
General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther..