Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.03 g/cc @Temperature 50.0 °C |
0.0372 lb/in³ @Temperature 122 °F |
Concentration 0.32 kg FeCl3/kg |
Solvay Chemicals Ferric chloride Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay |
|||
Density | 1.03 g/cc @Temperature 21.0 °C |
0.0372 lb/in³ @Temperature 69.8 °F |
|
BASF Pluracol® 1026 Molded Foam Polyol Description: Pluracol® 1026 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams. HR foams made with Pluracol 1026 in combination with graft polyols.. |
|||
Density | 1.03 g/cc @Temperature 40.0 °C |
0.0372 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 1365 Graft Slabstock Foam Polyol Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with.. |
|||
Density | 1.03 g/cc @Temperature 26.7 °C |
0.0372 lb/in³ @Temperature 80.1 °F |
|
BASF Pluracol® 355 Specialty Polyol Description: Pluracol® 355 polyol is an amine-based tetrol of low equivalent weight with built-in catalytic activity. Because of its unusual behavior, this polyol has found wide application in flex.. |
|||
Density | 1.03 g/cc @Temperature 40.0 °C |
0.0372 lb/in³ @Temperature 104 °F |
|
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p.. |
|||
Density | 1.03 g/cc @Temperature 60.0 °C |
0.0372 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 736 Rigid Polyol Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip.. |
|||
Density | 1.03 g/cc @Temperature 48.9 °C |
0.0372 lb/in³ @Temperature 120 °F |
|
BASF Pluracol® GP 430R Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Density | 1.03 g/cc @Temperature 70.0 °C |
0.0372 lb/in³ @Temperature 158 °F |
|
BASF Pluracol® 5250 Graft Slabstock Foam Polyol Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is .. |
|||
Density | 1.03 g/cc @Temperature 25.0 °C |
0.0372 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 628 Specialty Polyol Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used .. |
|||
Density | 1.03 g/cc @Temperature 37.8 °C |
0.0372 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® GP 730 Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Density | 1.03 g/cc @Temperature 25.0 °C |
0.0372 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® TP 440 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Density | 1.03 g/cc @Temperature 25.0 °C |
0.0372 lb/in³ @Temperature 77.0 °F |
|
BASF Quadrol® Specialty Polyol Description: Quadrol® polyol is N, N, N´, N´-Tetrakis (2-hydroxypropyl) ethylene-diamine. Quadrol has proven to be an excellent cross-linking agent and catalyst for use in polyurethane coatings a.. |