BASF Pluracol® 5250 Graft Slabstock Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 5250 Graft Slabstock Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is a stable heterogeneous dispersion which does not separate under normal storage conditions. Pluracol 5250 may be used alone or in combination with conventional polyols to increase load-bearing properties of flexible foams.Information provided by BASF
Physical Properties Metric English Comments
Density 1.03 g/cc

@Temperature 70.0 °C
0.0372 lb/in³

@Temperature 158 °F
1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
1.05 g/cc

@Temperature 25.0 °C
0.0379 lb/in³

@Temperature 77.0 °F
Viscosity 755 cP

@Temperature 70.0 °C
755 cP

@Temperature 158 °F
2520 cP

@Temperature 40.0 °C
2520 cP

@Temperature 104 °F
5820 cP

@Temperature 25.0 °C
5820 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.015
<= 0.015
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color White Opaque Liquid
Hydroxyl Number 23 - 26 mg KOH/g
STI 3007/3162