Material Notes:
Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with high load bearing and low resilience properties. These characteristics are advantageous in specialty packaging applications. Pluracol 1365 is not recommended for cushioning applications requiring high flex life due to the low resilience properties.Information provided by BASF
Physical Properties Metric English Comments
Density 1.03 g/cc

@Temperature 40.0 °C
0.0372 lb/in³

@Temperature 104 °F
1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
1.04 g/cc

@Temperature 30.0 °C
0.0376 lb/in³

@Temperature 86.0 °F
Viscosity 1680 cP

@Temperature 40.0 °C
1680 cP

@Temperature 104 °F
2560 cP

@Temperature 30.0 °C
2560 cP

@Temperature 86.0 °F
3260 cP

@Temperature 25.0 °C
3260 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color White Opaque Liquid
Hydroxyl Number 67 - 75 mg KOH/g
STI 3007/3162