BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor package. Pluracol 4850 can be used in combination with Pluracol 2100 to produce HR slabstock foams having a narrow spread in cross-sectional density and IFD properties and allows foam manufacturers to adjust the solids levels to specific formulations. Broad processing latitude permits the manufacture of a wide variety of high resilient foams. Pluracol 4850 polyol can also be used in molded foam applications.Information provided by BASF
Physical Properties Metric English Comments
Density 1.03 g/cc

@Temperature 40.0 °C
0.0372 lb/in³

@Temperature 104 °F
1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
Viscosity 1620 cP

@Temperature 40.0 °C
1620 cP

@Temperature 104 °F
2950 cP

@Temperature 25.0 °C
2950 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Creamy, Opaque Liquid
Hydroxyl Number 23 - 26 mg KOH/g
STI 3007/3162