Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Ferric chloride

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Ferric chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay
Physical Properties Metric English Comments
Density 0.970 g/cc

@Temperature 100 °C
0.0350 lb/in³

@Temperature 212 °F
Concentration 0.01 kg FeCl3/kg
0.997 g/cc

@Temperature 50.0 °C
0.0360 lb/in³

@Temperature 122 °F
Concentration 0.01 kg FeCl3/kg
1.002 g/cc

@Temperature 100 °C
0.03620 lb/in³

@Temperature 212 °F
Concentration 0.04 kg FeCl3/kg
1.009 g/cc

@Temperature 0.000 °C
0.03645 lb/in³

@Temperature 32.0 °F
Concentration 0.01 kg FeCl3/kg
1.024 g/cc

@Temperature 50.0 °C
0.03699 lb/in³

@Temperature 122 °F
Concentration 0.04 kg FeCl3/kg
1.03 g/cc

@Temperature 50.0 °C
0.0372 lb/in³

@Temperature 122 °F
Concentration 0.32 kg FeCl3/kg
1.036 g/cc

@Temperature 0.000 °C
0.03743 lb/in³

@Temperature 32.0 °F
Concentration 0.04 kg FeCl3/kg
1.039 g/cc

@Temperature 100 °C
0.03754 lb/in³

@Temperature 212 °F
Concentration 0.08 kg FeCl3/kg
1.057 g/cc

@Temperature 100 °C
0.03819 lb/in³

@Temperature 212 °F
Concentration 0.10 kg FeCl3/kg
1.06 g/cc

@Temperature 50.0 °C
0.0383 lb/in³

@Temperature 122 °F
Concentration 0.08 kg FeCl3/kg
1.072 g/cc

@Temperature 0.000 °C
0.03873 lb/in³

@Temperature 32.0 °F
Concentration 0.08 kg FeCl3/kg
1.074 g/cc

@Temperature 100 °C
0.03880 lb/in³

@Temperature 212 °F
Concentration 0.12 kg FeCl3/kg
1.078 g/cc

@Temperature 50.0 °C
0.03895 lb/in³

@Temperature 122 °F
Concentration 0.10 kg FeCl3/kg
1.09 g/cc

@Temperature 0.000 °C
0.0394 lb/in³

@Temperature 32.0 °F
Concentration 0.10 kg FeCl3/kg
1.097 g/cc

@Temperature 50.0 °C
0.03963 lb/in³

@Temperature 122 °F
Concentration 0.12 kg FeCl3/kg
1.108 g/cc

@Temperature 100 °C
0.04003 lb/in³

@Temperature 212 °F
Concentration 0.16 kg FeCl3/kg
1.109 g/cc

@Temperature 0.000 °C
0.04007 lb/in³

@Temperature 32.0 °F
Concentration 0.12 kg FeCl3/kg
1.135 g/cc

@Temperature 50.0 °C
0.04100 lb/in³

@Temperature 122 °F
Concentration 0.16 kg FeCl3/kg
1.142 g/cc

@Temperature 100 °C
0.04126 lb/in³

@Temperature 212 °F
Concentration 0.20 kg FeCl3/kg
1.147 g/cc

@Temperature 0.000 °C
0.04144 lb/in³

@Temperature 32.0 °F
Concentration 0.16 kg FeCl3/kg
1.174 g/cc

@Temperature 50.0 °C
0.04241 lb/in³

@Temperature 122 °F
Concentration 0.20 kg FeCl3/kg
1.178 g/cc

@Temperature 100 °C
0.04256 lb/in³

@Temperature 212 °F
Concentration 0.24 kg FeCl3/kg
1.187 g/cc

@Temperature 0.000 °C
0.04288 lb/in³

@Temperature 32.0 °F
Concentration 0.20 kg FeCl3/kg
1.215 g/cc

@Temperature 50.0 °C
0.04389 lb/in³

@Temperature 122 °F
Concentration 0.24 kg FeCl3/kg
1.216 g/cc

@Temperature 100 °C
0.04393 lb/in³

@Temperature 212 °F
Concentration 0.28 kg FeCl3/kg
1.229 g/cc

@Temperature 0.000 °C
0.04440 lb/in³

@Temperature 32.0 °F
Concentration 0.24 kg FeCl3/kg
1.237 g/cc

@Temperature 100 °C
0.04469 lb/in³

@Temperature 212 °F
Concentration 0.30 kg FeCl3/kg
1.258 g/cc

@Temperature 50.0 °C
0.04545 lb/in³

@Temperature 122 °F
Concentration 0.28 kg FeCl3/kg
1.259 g/cc

@Temperature 100 °C
0.04548 lb/in³

@Temperature 212 °F
Concentration 0.32 kg FeCl3/kg
1.274 g/cc

@Temperature 0.000 °C
0.04603 lb/in³

@Temperature 32.0 °F
Concentration 0.28 kg FeCl3/kg
1.28 g/cc

@Temperature 50.0 °C
0.0462 lb/in³

@Temperature 122 °F
Concentration 0.30 kg FeCl3/kg
1.298 g/cc

@Temperature 0.000 °C
0.04689 lb/in³

@Temperature 32.0 °F
Concentration 0.30 kg FeCl3/kg
1.311 g/cc

@Temperature 100 °C
0.04736 lb/in³

@Temperature 212 °F
Concentration 0.36 kg FeCl3/kg
1.322 g/cc

@Temperature 0.000 °C
0.04776 lb/in³

@Temperature 32.0 °F
Concentration 0.32 kg FeCl3/kg
1.351 g/cc

@Temperature 50.0 °C
0.04881 lb/in³

@Temperature 122 °F
Concentration 0.36 kg FeCl3/kg
1.373 g/cc

@Temperature 0.000 °C
0.04960 lb/in³

@Temperature 32.0 °F
Concentration 0.36 kg FeCl3/kg
1.376 g/cc

@Temperature 100 °C
0.04971 lb/in³

@Temperature 212 °F
Concentration 0.40 kg FeCl3/kg
1.402 g/cc

@Temperature 50.0 °C
0.05065 lb/in³

@Temperature 122 °F
Concentration 0.40 kg FeCl3/kg
1.40 - 1.45 g/cc

@Temperature 20.0 °C
0.0506 - 0.0524 lb/in³

@Temperature 68.0 °F
MG 1001
1.43 g/cc

@Temperature 0.000 °C
0.0517 lb/in³

@Temperature 32.0 °F
Concentration 0.40 kg FeCl3/kg
1.457 g/cc

@Temperature 50.0 °C
0.05264 lb/in³

@Temperature 122 °F
Concentration 0.44 kg FeCl3/kg
1.463 g/cc

@Temperature 100 °C
0.05285 lb/in³

@Temperature 212 °F
Concentration 0.44 kg FeCl3/kg
1.492 g/cc

@Temperature 0.000 °C
0.05390 lb/in³

@Temperature 32.0 °F
Concentration 0.44 kg FeCl3/kg
pH 1.0 - 1.4
1.0 - 1.4
Viscosity 0.287 cP

@Temperature 100 °C
0.287 cP

@Temperature 212 °F
Dynamic, Concentration 0.01 kg FeCl3/kg
0.311 cP

@Temperature 100 °C
0.311 cP

@Temperature 212 °F
Dynamic, Concentration 0.04 kg FeCl3/kg
0.349 cP

@Temperature 100 °C
0.349 cP

@Temperature 212 °F
Dynamic, Concentration 0.08 kg FeCl3/kg
0.371 cP

@Temperature 100 °C
0.371 cP

@Temperature 212 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
0.395 cP

@Temperature 100 °C
0.395 cP

@Temperature 212 °F
Dynamic, Concentration 0.12 kg FeCl3/kg
0.449 cP

@Temperature 100 °C
0.449 cP

@Temperature 212 °F
Dynamic, Concentration 0.16 kg FeCl3/kg
0.512 cP

@Temperature 100 °C
0.512 cP

@Temperature 212 °F
Dynamic, Concentration 0.20 kg FeCl3/kg
0.564 cP

@Temperature 50.0 °C
0.564 cP

@Temperature 122 °F
Dynamic, Concentration 0.01 kg FeCl3/kg
0.586 cP

@Temperature 100 °C
0.586 cP

@Temperature 212 °F
Dynamic, Concentration 0.24 kg FeCl3/kg
0.628 cP

@Temperature 50.0 °C
0.628 cP

@Temperature 122 °F
Dynamic, Concentration 0.04 kg FeCl3/kg
0.673 cP

@Temperature 100 °C
0.673 cP

@Temperature 212 °F
Dynamic, Concentration 0.28 kg FeCl3/kg
0.722 cP

@Temperature 100 °C
0.722 cP

@Temperature 212 °F
Dynamic, Concentration 0.30 kg FeCl3/kg
0.737 cP

@Temperature 50.0 °C
0.737 cP

@Temperature 122 °F
Dynamic, Concentration 0.08 kg FeCl3/kg
0.775 cP

@Temperature 100 °C
0.775 cP

@Temperature 212 °F
Dynamic, Concentration 0.32 kg FeCl3/kg
0.802 cP

@Temperature 50.0 °C
0.802 cP

@Temperature 122 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
0.874 cP

@Temperature 50.0 °C
0.874 cP

@Temperature 122 °F
Dynamic, Concentration 0.12 kg FeCl3/kg
0.894 cP

@Temperature 100 °C
0.894 cP

@Temperature 212 °F
Dynamic, Concentration 0.36 kg FeCl3/kg
1.033 cP

@Temperature 100 °C
1.033 cP

@Temperature 212 °F
Dynamic, Concentration 0.40 kg FeCl3/kg
1.044 cP

@Temperature 50.0 °C
1.044 cP

@Temperature 122 °F
Dynamic, Concentration 0.16 kg FeCl3/kg
1.196 cP

@Temperature 100 °C
1.196 cP

@Temperature 212 °F
Dynamic, Concentration 0.44 kg FeCl3/kg
1.253 cP

@Temperature 50.0 °C
1.253 cP

@Temperature 122 °F
Dynamic, Concentration 0.20 kg FeCl3/kg
Copyright © lookpolymers.com All Rights Reserved