Material Notes:
Description: Quadrol® polyol is N, N, N´, N´-Tetrakis (2-hydroxypropyl) ethylene-diamine. Quadrol has proven to be an excellent cross-linking agent and catalyst for use in polyurethane coatings and rigid foams. The four hydroxyl groups in Quadrol give multiple cross-linking sites and the two tertiary nitrogen atoms provide catalysis for the reaction.Information provided by BASF
Physical Properties Metric English Comments
Density 1.01 g/cc

@Temperature 60.0 °C
0.0365 lb/in³

@Temperature 140 °F
1.02 g/cc

@Temperature 40.0 °C
0.0368 lb/in³

@Temperature 104 °F
1.03 g/cc

@Temperature 25.0 °C
0.0372 lb/in³

@Temperature 77.0 °F
Viscosity 900 cP

@Temperature 60.0 °C
900 cP

@Temperature 140 °F
10000 cP

@Temperature 40.0 °C
10000 cP

@Temperature 104 °F
52000 cP

@Temperature 25.0 °C
52000 cP

@Temperature 77.0 °F
Molecular Weight 292 g/mol
292 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
STI 3062
Descriptive Properties Value Comments
Assay >99%
STI 4086
Color <70
APHA, STI 3057
Water White Liquid
Hydroxyl Number 770 mg KOH/g