BASF Pluracol® 1026 Molded Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 1026 Molded Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 1026 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams. HR foams made with Pluracol 1026 in combination with graft polyols, such as Pluracol 973, process well and are easily crushed.Information provided by BASF
Physical Properties Metric English Comments
Density 0.997 g/cc

@Temperature 48.9 °C
0.0360 lb/in³

@Temperature 120 °F
1.01 g/cc

@Temperature 37.8 °C
0.0365 lb/in³

@Temperature 100 °F
1.03 g/cc

@Temperature 21.0 °C
0.0372 lb/in³

@Temperature 69.8 °F
Viscosity 350 cP

@Temperature 48.9 °C
350 cP

@Temperature 120 °F
650 cP

@Temperature 37.8 °C
650 cP

@Temperature 100 °F
1329 cP

@Temperature 21.0 °C
1329 cP

@Temperature 69.8 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 26.5 - 28.5 mg KOH/g
STI 3007/3162
Unsaturation <0.06 meq/g
STI 3056