Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stability. This material is an excellent choice for the molding of intricate patterns which involve deep undercuts and where dimensional stability becomes important while maintaining fairly low modulus. A variety of catalysts are offered with this material. Complies with FDA indirect food contact regulation CFR 177.2600 when used with Cat Clear FG. Refer to Cat Clear FG data sheet for specific properties.Key Features: Low viscosity Excellent tear resistance Fast demold time Moderately high durometer with a moderately low modulusMain Applications: Molds for small statues, large statues and monument restoration Molds for polyester, polyurethane and epoxy resin castings Molds for prototypes Picture frame and architectural moldsPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Uncatalyzed, QM CAT PURPLE
1.00 g/cc
1.00 g/cc
Uncatalyzed, QM CAT PURPLE
1.03 g/cc
1.03 g/cc
Uncatalyzed, QM CAT BLUE
1.25 g/cc
1.25 g/cc
catalyzed with QM CAT PURPLE
1.25 g/cc
1.25 g/cc
catalyzed with QM CAT RED 3
1.25 g/cc
1.25 g/cc
catalyzed with QM CAT BLUE
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT PURPLE
100 cP
100 cP
Uncatalyzed, QM CAT BLUE
100 cP
100 cP
Uncatalyzed, QM CAT RED 3
15000 cP
15000 cP
catalyzed with QM CAT RED 3
15000 cP
15000 cP
catalyzed with QM CAT BLUE
15000 cP
15000 cP
catalyzed with QM CAT PURPLE
25000 cP
25000 cP
Base
Linear Mold Shrinkage <= 0.0030 cm/cm
<= 0.0030 in/in
cured 72 hrs @ RT
Storage Temperature <= 38.0 °C
<= 100 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 22
22
cured 72 hrs @ RT
Tensile Strength, Yield 2.76 MPa
400 psi
cured 72 hrs @ RT
Elongation at Break 300 %
300 %
cured 72 hrs @ RT
Tear Strength 20.2 kN/m
115 pli
cured 72 hrs @ RT
Processing Properties Metric English Comments
Dry Time 4 - 6 hour
4 - 6 hour
Demold time, catalyzed with QM CAT RED 3
12 - 16 hour
12 - 16 hour
Demold time, catalyzed with QM CAT PURPLE
16 - 24 hour
16 - 24 hour
Demold time, catalyzed with QM CAT BLUE
Cure Time 45.0 - 60.0 min
0.750 - 1.00 hour
Tack Free Time, catalyzed with QM CAT RED 3
240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
360 - 480 min
6.00 - 8.00 hour
Tack Free Time, catalyzed with QM cat BLUE
Descriptive Properties Value Comments
Color Beige
Base
Blue
Uncatalyzed, QM CAT BLUE
Light Blue
catalyzed with QM CAT BLUE
Light Purple
catalyzed with QM CAT PURPLE
Light Red
catalyzed with QM CAT RED 3
Purple
Uncatalyzed, QM CAT PURPLE
Red
Uncatalyzed, QM CAT RED 3
Work Life 35 mins
catalyzed with QM CAT PURPLE
45 mins
catalyzed with QM CAT BLU
7 mins
catalyzed with QM CAT RED 3
Copyright © lookpolymers.com All Rights Reserved