ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM 264 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 264 is exceptionally good where high durometer and dimensional stability are required. Material complies with FDA indirect food contact regulation CFR 177.2600.Key Features: High Durometer Casting resin resistance Fast demold time Excellent dimensional stability Main Applications: Molds for architectural replication Molds for polyester, epoxy resin casting, and rigid or foam polyurethane Molds for technical articles and prototype Molds for furniture and picture frame replication Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Uncatalyzed, QM 264B
1.28 g/cc
1.28 g/cc
Base
Viscosity 5200 cP
5200 cP
Uncatalyzed, QM 264B
110000 cP
110000 cP
catalyzed with QM 264B
150000 cP
150000 cP
Base
Linear Mold Shrinkage <= 0.0010 cm/cm
<= 0.0010 in/in
cured 72 hrs @ RT
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
cured 72 hrs @ RT
Tensile Strength, Yield 5.50 MPa
798 psi
cured 72 hrs @ RT
Elongation at Break 240 %
240 %
cured 72 hrs @ RT
Tear Strength 21.0 kN/m
120 pli
cured 72 hrs @ RT
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Dry Time 12 - 18 hour
12 - 18 hour
Demold time, catalyzed with QM 264B
Descriptive Properties Value Comments
Color Beige
Base
Blue
Uncatalyzed, QM 264B
Light Blue
catalyzed with QM 264B
Work Life 75 mins
catalyzed with QM 264B