ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QLE 1031 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: 100% solids Long open time Excellent adhesion Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
"B" component
1.18 g/cc
1.18 g/cc
"A" component
Viscosity 1200 cP
1200 cP
"B" component
25000 cP
25000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
cured 20 mins @150°C
Tensile Strength, Yield 1.70 MPa
247 psi
cured 20 mins @150°C
Elongation at Break 150 %
150 %
cured 20 mins @150°C
Processing Properties Metric English Comments
Gel Time >= 4320 min
>= 4320 min
Catalyzed
Descriptive Properties Value Comments
Color Clear
"B" component
White
"A" component