Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Load Melt Index = 10 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 240 °C
10 g/10 min

@Load 47.6 lb,
Temperature 464 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PPE 1461  (discontinued **)
PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete  (disc
Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resinCharacteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248;..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE  (discontinued **)
Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes..
High Load Melt Index 10 g/10 min
10 g/10 min
ASTM D1238
Ineos G36-10-150 HDPE
G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes...
High Load Melt Index 10 g/10 min
10 g/10 min
ASTM D1238
Ineos G50-100 HDPE
Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p..
High Load Melt Index 10 - 14 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 - 14 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GM 8260 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
at listed melt temp
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis BorPEX™ HE1878E High Density Polyethylene Powder for Crosslinked Pipes
BorPEX HE1878E is a high molecular weight, high density polyethylene powder specially designed for production of peroxide crosslinked pipes (PEX pipes).Crosslinked (PEX) pipes based on BorPEX HE1878..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
BorPEXME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation c..
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
ASTM D 1238
Total 2287 HDPE Bimodal Film Resin
Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe..
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
ISO 1133
Total HP 401 MDPE, pipe, cable, sheet
FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55..
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
ASTM D1238
Equate EGDA-6888 HDPE Film Extrusion Resin
EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee..
High Load Melt Index 10 g/10 min

@Load 21.0 kg
10 g/10 min

@Load 46.3 lb
ASTM D1238
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HD 7960.13 HMW Blown Film Resin
Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 ..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Dow UNIPOL™ DGDA-5110 Polyolefin
DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis BorPEX™ HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation))
BorPEX HE2591 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, offering excellent processability for peroxide crosslinking. It is a special polymer, stabilized ..
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Formosa Plastics Formolene® HL5010 Blow Molding HDPE
Extra High Molecular Weight Hexene CopolymerApplications: Blow Molded 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks; Extruded pallets, cattle feeders, large formed parts..
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
ASTM D 1238
Total Finathene® CD 481 HDPE conduit  (discontinued **)
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.