Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. These properties make Formolene® HL5010 an excellent resin for large part blow molding applications. Formolene® HL5010 meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 for food packaging, covering safe use of polyolefin articles intended for direct food contact.Applications: Blow Molded - 55-Gallon Shipping Containers, Gasoline Tanks and Agricultural Chemical Tanks; Extruded – Pallets, Cattle Feeders, Large Formed Parts and BoatsInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 600 hour
>= 600 hour
Condition A, F<sub>50</sub>; ASTM D1693
ESCR 10% Igepal® >= 600 hour
>= 600 hour
Condition B, F<sub>50</sub>; ASTM D1693
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 600 %
>= 600 %
2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -91.0 °C
<= -132 °F
ASTM D746