Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos G36-10-150 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos G36-10-150 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D4883 (Natural)
Environmental Stress Crack Resistance >= 3000 hour
>= 3000 hour
Single Point Method; ASTM D5397
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
200°C
High Load Melt Index 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 17.2 MPa
2490 psi
2 in/min.; ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min.; ASTM D638
Flexural Modulus 0.655 GPa
95.0 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 6.00 J/cm
11.2 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D 746
Descriptive Properties Value Comments
Process Extrusion
Users viewing this material also viewed the following: