Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 8.0 - 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.0 - 14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 5010 T2 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 10 - 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 - 14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 8.0 - 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.0 - 14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 9245 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 8.0 - 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.0 - 14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |