Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.942 - 0.946 g/cc
0.0340 - 0.0342 lb/in³
Base Resin; ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D1693
Melt Flow 0.60 - 0.80 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.60 - 0.80 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
10.8 - 14.4 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.8 - 14.4 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 0.900 GPa
>= 131 ksi
ASTM D790
Izod Impact, Notched >= 3.00 J/cm

@Temperature 23.0 °C
>= 5.62 ft-lb/in

@Temperature 73.4 °F
ASTM D256