Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MTM Plastics Purpolen® PE Polyethylene Regrind

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer MTM Plastics GmbH
Trade Name Purpolen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MTM Plastics Purpolen® PE Polyethylene Regrind.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® is a pre-product sorted according to type and color, which is produced through a patented separating process.Information provided by MTM Plastics GmbH.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Moisture Absorption <= 0.100 %
<= 0.100 %
Melt Flow <= 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
<= 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
<= 1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
<= 3.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
<= 3.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
Ignition Residue after 650°C; ISO 1172
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
DIN 53505
Tensile Strength, Yield >= 23.0 MPa
>= 3340 psi
50 mm/min; ISO 527
Elongation at Yield >= 75 %
>= 75 %
50 mm/min; ISO 527
Tensile Modulus >= 0.850 GPa
>= 123 ksi
1 mm/min; ISO 527
Charpy Impact, Notched >= 0.600 J/cm²

@Temperature -23.0 °C
>= 2.86 ft-lb/in²

@Temperature -9.40 °F
edgewise; ISO 179
>= 3.00 J/cm²

@Temperature 23.0 °C
>= 14.3 ft-lb/in²

@Temperature 73.4 °F
edgewise; ISO 179
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved