Polymer Property : Thickness = 7.87 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep..
Thickness 175 - 200 microns
6.89 - 7.87 mil
Parker Chomerics WIN-SHIELD® AgF8 Conductive Film
Description: Chomerics’ AgF8 conductive film is a multi-layer, silver oxide-based thin film coating applied to a heat stabilized, optical quality polyester film AgF8 film-provides high visible ligh..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile ..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Thickness 30.0 - 200 microns
1.18 - 7.87 mil
possible range, depending on extrusion conditions
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Bapolene® 105F Low Density Polyethylene Film Resin
Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th..
Thickness 120 - 200 microns
4.72 - 7.87 mil
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Thickness 120 - 200 microns
4.72 - 7.87 mil
Beijing Evergrow Resources CFC-DD-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Thickness 120 - 200 microns
4.72 - 7.87 mil
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40006T/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40006T/4
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40009.5S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40012T/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40036S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40054V/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40406B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40810B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-41014B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-42424B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-43036B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-80036S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 120 - 200 microns
4.72 - 7.87 mil
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40054V/m
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..