Physical Properties Metric English Comments
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40006T/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40006T/4
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40009.5S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40012T/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40036S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40054V/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40406B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40810B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-41014B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-42424B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-43036B
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-80036S/2
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Thickness 65.0 microns
2.56 mil
Total Thickness
Caplinq LINQTAPE™ PIT1A
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Thickness 65.0 microns
2.56 mil
Total Thickness
Caplinq LINQTAPE™ PIT1S
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Thickness 65.0 - 200 microns
2.56 - 7.87 mil
Caplinq LINQSTAT™ VCF-40054V/m
Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni..
Copyright © lookpolymers.com All Rights Reserved