Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.0 microns | 1.18 mil | |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 30.0 microns | 1.18 mil | Recommended |
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 30 µm) PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 30 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | As Tested |
Solvay Specialty Polymers Ajedium™ Films -- Udel® PSU P-1700 NT-11 Polysulfone (PSU) Udel® P-1700 polysulfones are tough, high-strength thermoplastics that are suitable for continuous use up to 300°F (149°C). Udel Film is resistant to oxidation and hydrolysis and withstand .. |
|||
Thickness | 30.0 - 200 microns | 1.18 - 7.87 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
ExxonMobil Hicor® 30 HT 103 OHD Film One-side treated, non-sealable, oriented high density polyethylene film, which has outstanding stiffness, deadfold, and directional tear characteristics. This film has been designed to be used in va.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
ExxonMobil Hicor® 30 HT 183 OHD Film One-side metallized, non-sealable, oriented high density polyethylene film, which has outstanding deadfold and directional tear characteristics. This film has been designed to be used in various app.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |