Parker Chomerics WIN-SHIELD® AgF8 Conductive Film

Category Polymer , Film
Manufacturer Parker Chomerics
Trade Name WIN-SHIELD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics WIN-SHIELD® AgF8 Conductive Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chomerics’ AgF8 conductive film is a multi-layer, silver oxide-based thin film coating applied to a heat stabilized, optical quality polyester film AgF8 film-provides high visible light transmission and significant infrared reflectance. The silver coating also provides high electrical conductivity, making AgF8 film a good EMI shielding material from 1 MHz to 1 GHz, suitable for use in most display applications. AgF8 conductive film is an ideal EMI shielding medium for applications where optical quality cannot be specified. Examples include high resolution CRT displays, multi-color displays, LCDs and EL displays. AgF8 conductive film will reflect heat for temperature-sensitive LCD applications.Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 175 - 200 microns
6.89 - 7.87 mil
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Typical
20 %

@Wavelength 1500 nm
20 %

@Wavelength 1500 nm
74% Reflection
35 %

@Wavelength 1200 nm
35 %

@Wavelength 1200 nm
55% Reflection
60 %

@Wavelength 400 nm
60 %

@Wavelength 400 nm
10% Reflection
76 %

@Wavelength 650 nm
76 %

@Wavelength 650 nm
10% Reflection
80 %

@Wavelength 600 nm
80 %

@Wavelength 600 nm
6% Reflection
82 %

@Wavelength 500 nm
82 %

@Wavelength 500 nm
6% Reflection
82 %

@Wavelength 550 nm
82 %

@Wavelength 550 nm
5% Reflection
Electrical Properties Metric English Comments
Surface Resistivity per Square 8.0 - 12 ohm
8.0 - 12 ohm
Shielding Effectiveness 18 dB

@Frequency 1.00e+10 Hz
18 dB

@Frequency 1.00e+10 Hz
Plane Wave
24 dB

@Frequency 1.00e+9 Hz
24 dB

@Frequency 1.00e+9 Hz
Plane Wave
54 dB

@Frequency 1.00e+8 Hz
54 dB

@Frequency 1.00e+8 Hz
E-Field
60 dB

@Frequency 1.00e+7 Hz
60 dB

@Frequency 1.00e+7 Hz
E-Field
100 dB

@Frequency 1.00e+6 Hz
100 dB

@Frequency 1.00e+6 Hz
E-Field
Descriptive Properties Value Comments
Environmental Stability 120 hrs with no change in resistance
Humidity: 60°C, 95% RH
120 hrs with no change in resistance
Dry Heat: 100°C
120 hrs with no change in resistance
Saturated NaCl