Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.0 microns | 1.18 mil | |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 120W Linear Low Density Polyethylene for Blown Film Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Thickness | 30.0 - 150 microns | 1.18 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 30.0 - 50.0 microns | 1.18 - 1.97 mil | |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Thickness | 30.0 microns | 1.18 mil | |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSD11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dim.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 30 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSS11 Normal Grade Heat Sealable Film (thickness: 30 µm) HSS11 is a general, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimens.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Thickness | 30.0 microns | 1.18 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG11 Bag Grade BOPP Plain Film (thickness: 30 µm) PG11 is a general, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness, and one side has corona treatment. It is widely used in gift wrapping, textiles, and.. |
|||
Thickness | 30.0 - 120 microns | 1.18 - 4.72 mil | |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2070126D4 High Brightness Phosphor Ink (Orange) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured film thickness, on 175µm ITO coated polyester |
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2070209P5 High Brightness Phosphor Ink (Green) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact .. |
|||
Thickness | 30.0 microns | 1.18 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Thickness | 30.0 microns | 1.18 mil | Cured thickness on 175µm ITO coated polyester |
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Thickness | 30.0 - 1100 microns | 1.18 - 43.3 mil | |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Thickness | 30.0 - 300 microns | 1.18 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Thickness | 30.0 - 200 microns | 1.18 - 7.87 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 35 is made by a high pressure tubular process. Grade for flexible films, with high transparency and outstanding mechanical properties. Contains NO antioxidant.Information provided by T.. |
|||
Thickness | 30.0 - 300 microns | 1.18 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Thickness | 30.0 microns | 1.18 mil | |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |