Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 30.0 - 100 microns | 1.18 - 3.94 mil | Recommended |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | possible range, depending on extrusion conditions |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Thickness | 20.0 - 100 microns | 0.787 - 3.94 mil | possible range, depending on extrusion conditions |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Thickness | 15.0 - 100 microns | 0.591 - 3.94 mil | possible range, depending on extrusion conditions |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |