Bapolene® 350F Polyethylene, Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 350F Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Blown film extrusion of T-shirt sacks, merchandise bags.Film properties below are based on a thickness of .8 mil and blow-up ratio of 4:1.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Thickness 20.0 microns
0.787 mil
4:1 blow-up ratio
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
High Load Melt Index 6.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
>200; ASTM D-882, A
Film Elongation at Break, TD 200 %
200 %
>200; ASTM D-882, A
Elmendorf Tear Strength, MD 1.08 g/micron
27.4 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 6.20 g/micron
157 g/mil
ASTM D-1922
Dart Drop 12.8 g/micron
325 g/mil
ASTM D-1709
Film Tensile Strength at Break, MD 52.0 MPa
7540 psi
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
Descriptive Properties Value Comments
Process Blown Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution