Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and good gauge control. The combination of these features ensures films with outstanding optical properties and excellent impact and tear resistance.Lumicene® mPE M 2735 S01 is suited for many applications in the field of cast film, stretch wrap film (low cling), hygiene film (f.e.. diaper backsheet), lamination and artificial grass.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.927 g/cc
0.927 g/cc
ISO 1183
Thickness 20.0 microns
0.787 mil
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.00 MPa
1310 psi
ISO 527-3
Film Tensile Strength at Yield, TD 9.00 MPa
1310 psi
ISO 527-3
Film Elongation at Break, MD 470 %
470 %
ISO 527-3
Film Elongation at Break, TD 530 %
530 %
ISO 527-3
Elmendorf Tear Strength, MD 5.10 g/micron
130 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 12.2 g/micron
310 g/mil
ISO 6383-2
Dart Drop Test 100 g
0.221 lb
ISO 7765-1
Film Tensile Strength at Break, MD 39.0 MPa
5660 psi
ISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa
3480 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
ISO 11357
Vicat Softening Point 118 °C
244 °F
ISO 306
Optical Properties Metric English Comments
Haze 1.3 %
1.3 %
ISO 14782
Gloss 89 %
89 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Chill Roll
Melt Temperature 240 - 280 °C
464 - 536 °F
Users viewing this material also viewed the following: