Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Film
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability. It is also biologically and chemically inert.The NOVA Chemicals Material Safety Data Sheet contains important safety information and should be reviewed before using the product.Features: Excellent stiffness and glossAdditives: High temperature AOApplications: Blending, Co-extruded filmsFilm properties are Typical of cast film extruded at 280°C.
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ASTM D 792
Thickness 20.0 microns
0.787 mil
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 15.0 MPa
2180 psi
ASTM D 882
Film Tensile Strength at Yield, TD 15.0 MPa
2180 psi
ASTM D 882
Film Elongation at Break, MD 600 %
600 %
ASTM D 882
Film Elongation at Break, TD 900 %
900 %
ASTM D 882
Elmendorf Tear Strength MD 19 g
19 g
ASTM D 1922
Elmendorf Tear Strength TD 320 g
320 g
ASTM D 1922
Elmendorf Tear Strength, MD 0.950 g/micron
24.1 g/mil
ASTM D 1922
Elmendorf Tear Strength, TD 16.0 g/micron
406 g/mil
ASTM D 1922
Film Tensile Strength at Break, MD 38.0 MPa
5510 psi
ASTM D 882
Film Tensile Strength at Break, TD 26.0 MPa
3770 psi
ASTM D 882
1% Secant Modulus, MD 340 MPa
49300 psi
ASTM D 882
1% Secant Modulus, TD 430 MPa
62400 psi
ASTM D 882
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D 1003
Gloss 88 %
88 %
45°; ASTM D 2457
Descriptive Properties Value Comments
Low Friction Puncture 3 (ft-lb/mil)
NOVA Chemicals test method
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved