Tipco Tipcolene® DR 8201 - 20% Talc/Mineral Reinforced, Impact Modified, Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® DR 8201 - 20% Talc/Mineral Reinforced, Impact Modified, Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break >= 75 %
>= 75 %
ASTM D638
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
253 °F
ASTM D648