Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 50265-2-1 requirement. 88 Shore A hardness. Processing typically conducted on standard extrusion equipment. Wire tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 10.0 kg,
Temperature 250 °C
9.0 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
30S reading; ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
50 mm/min; ISO 527
13.0 MPa
1890 psi
Type I, 50 mm/min; ASTM D638
18.0 MPa
2610 psi
UL 1581
20.0 MPa
2900 psi
after 7days @80°C; UL 1581
Elongation at Break 200 %
200 %
Type I, 50 mm/min; ASTM D638
200 %
200 %
50 mm/min; ISO 527
226 %
226 %
after 7days @136°C; UL 1581
248 %
248 %
UL 1581
Flexural Modulus 0.0400 GPa
5.80 ksi
12.5 mm/min; ISO 178
0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
Heat Distortion 13 %

@Load 0.250 kg,
Temperature 100 °C
13 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 34 %
34 %
ISO 4589
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 5.20e+15 ohm-cm
5.20e+15 ohm-cm
ASTM D257
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 23.7 kV/mm

@Thickness 2.00 mm
602 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 71
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 165
ASTM E 662
Vertical Flame Test PASSES
EN 50265-2-1
Users viewing this material also viewed the following: