Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.011 - 0.020 cm/cm
0.011 - 0.020 in/in
ASTM D955
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 200 %
200 %
Type I, 51 mm/min; ASTM D638
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C

@Thickness 3.18 mm
203 °F

@Thickness 0.125 in
Annealed; ASTM D648
UL RTI, Mechanical without Impact 115 °C
239 °F
UL 746
Flammability, UL94 V-2

@Thickness 0.749 mm
V-2

@Thickness 0.0295 in
ALL; Internal Method
Oxygen Index 27 %

@Thickness 3.18 mm
27 %

@Thickness 0.125 in
ASTM D2863
Descriptive Properties Value Comments
Appearance Black
Colors Available
White
Features Flame Retardant
Medium Flow
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding