Material Notes:
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON D series consists of an unsaturated polymer, either butadiene or isoprene, as the rubber monomer. Information provided by the manufacturer, Kraton® Polymers.
Physical Properties Metric English Comments
Melt Flow 1.8 g/10 min
1.8 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.0 MPa
4350 psi
Tensile Strength, Yield 13.5 MPa
1960 psi
Flexural Modulus 0.600 GPa
87.0 ksi
Izod Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
NB

@Temperature 0.000 °C
NB

@Temperature 32.0 °F
3.2 mm (0.125 in) notch
Falling Dart Impact >= 244 J
>= 180 ft-lb
Falling weight impact at 23°C (73.4°F)