Material Notes:
Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Melt Flow 1.8 g/10 min
1.8 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.17 MPa
1180 psi
ASTM D412
Elongation at Break 711 %
711 %
ASTM D412
100% Modulus 0.00250 GPa
0.363 ksi
ASTM D412
300% Modulus 0.00120 GPa
0.174 ksi
ASTM D412
Tear Strength 34.1 kN/m
195 pli
ASTM D624