Material Notes:
F300 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.37 GPa
199 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525