Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The FP33 resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for film extrusion with good mechanical properties. It contains processing aid, slip, and antiblock additives. Its applications include thin films and automatic packaging which require higher stiffness: textile products, toilet paper, and others. Recommended film thickness: 0.025 to 0.100mm. The FP33 resin should be processed on specific extruders for LMDPE. The best results can be obtained with a temperature profile between 150 to 190º and blends with LDPE or MDPE using a ratio between 20% to 50%, allowing expressive improvement on optical properties.
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM-D792
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 990 %
990 %
ASTM-D882
Film Elongation at Break, TD 1440 %
1440 %
ASTM-D882
Elmendorf Tear Strength MD 20 g
20 g
ASTM-D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM-D1922
Elmendorf Tear Strength, MD 0.530 g/micron
13.5 g/mil
ASTM-D1922
Elmendorf Tear Strength, TD 4.74 g/micron
120 g/mil
ASTM-D1922
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM-D882
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
ASTM-D882
1% Secant Modulus, MD 320 MPa
46400 psi
ASTM-D882
1% Secant Modulus, TD 380 MPa
55100 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 44 %
44 %
ASTM-D1003
Gloss 45 %
45 %
Angle 60°; ASTM-D2457
Copyright © lookpolymers.com All Rights Reserved