Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 1200 cP @Temperature 23.0 °C |
1000 - 1200 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Clear 100 3D Printing Polymer Ultra clear.Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Wide range of medical applicationInformation provided by G.. |
|||
Viscosity | 900 - 1200 cP | 900 - 1200 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 160 (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 900 - 1200 cP | 900 - 1200 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 500 - 1200 cP @Temperature 25.0 °C |
500 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers MPC-023 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-071 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 - 1200 cP @Temperature 25.0 °C |
600 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PNC-153 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PPA-059 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 - 1200 cP @Temperature 25.0 °C |
600 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers YPX-164 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
Uncured |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Viscosity | 600 - 1200 cP @Temperature 71.1 °C |
600 - 1200 cP @Temperature 160 °F |
|
Northstar Polymers PAA-109 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 - 1200 cP | 600 - 1200 cP | |
Huntsman Araldite EPN 1138 MAK-80 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 175 to 181. Max color is 2.Comments/Applications: EPN 1138 80% solids in Methyl n-Amyl Ketone. High performance, chemically resistant tank linings, maintenance coati.. |
|||
Viscosity | 460 - 1200 cP | 460 - 1200 cP | |
Huntsman HY 3150 Aromatic Amine Approx. H+ equivalent weight 58. Mix Ratio with GY 6010 is 23.Comments/Applications: High solids coatings, floorings and tank linings. Good acetic acid resistance and other aggressive environment.. |
|||
Viscosity | 700 - 1200 cP | 700 - 1200 cP | |
Lucite International Colacryl ® TS1171/1 Acrylic Solution Resin Butyl methacrylate-Methyl methacrylate copolymerThis product is a fairly soft and flexible copolymer with reasonable abrasion resistance. It has good UV resistance and is therefore suitable for outd.. |
|||
Viscosity | 1000 - 1200 cP | 1000 - 1200 cP | B component |
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-626L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 500 - 1200 cP | 500 - 1200 cP | #2 SP. @30 RPM; RP-0659 |
Solvay ALKASPERSE® A-5H Surfactant Chemical Name: PARTIAL SODIUM SALT OF POLYACRYLIC ACIDCAS: 9003-01-4, 9003-04-7 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKASPERSE© A-5H is a solid disper.. |
|||
Viscosity | 400 - 1200 cP | 400 - 1200 cP | #3 SP @ 60 rpm; RP-0596 |
Solvay RHODOLINE® 622 Surfactant Description: Mineral oil based defoamers for flat to gloss paints, great process foam know down.Identification: OIL BASE DEFOAMERAvailable in: North AmericaSolubility: Not dispersible in waterApplic.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | #3 sp @ 60 rpm; RP-0596 |
Solvay RHODOLINE® 697 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Viscosity | 650 - 1200 cP @Temperature 125 °C |
650 - 1200 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Viscosity | 600 - 1200 cP | 600 - 1200 cP | Part B |
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Viscosity | 600 - 1200 cP | 600 - 1200 cP | NOV QC 020 |
Lubrizol ESTANE® 5722 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 700 - 1200 cP @Temperature 23.0 °C |
700 - 1200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Viscosity | 800 - 1200 cP @Temperature 23.0 °C |
800 - 1200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | |
Epoxyset Epoxibond EB-119M Unfilled Epoxy Adhesive A two-component,unfilled, low viscosity, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by.. |
|||
Viscosity | 1000 - 1200 cP @Temperature 60.0 °C |
1000 - 1200 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G200 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 800 - 1200 cP @Temperature 35.0 °C |
800 - 1200 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer Description: Used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 300 - 1200 cP | 300 - 1200 cP | #2 SP. @ 30 rpm; RP-0596 |
Solvay RHODAPEX® ESY/CG Surfactant I.N.C.I. Name: Sodium Laureth SulfateCAS: 68585-34-2Compatible with most surfactant solutions and water soluble polymers.Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio.. |