Aremco Crystalbond™ 555 Washaway Mounting Adhesive & Accessory

Category Polymer , Adhesive
Manufacturer Aremco
Trade Name Crystalbond™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Crystalbond™ 555 Washaway Mounting Adhesive & Accessory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low melting point adhesive systems for moderate-stress machining processes, dry plasma etching of silicon wafers and de-paneling copper plated Teflon boards. Transparent in thin cross-sections. Soluble in hot water.
Physical Properties Metric English Comments
Viscosity 500 cP
500 cP
Thermal Properties Metric English Comments
Liquidus 49.0 °C
120 °F
Flow Point
Descriptive Properties Value Comments
Color White
Solvent Hot Water