Solvay MACKAM® 2CSF-40CG Surfactant

Category Fluid
Manufacturer Solvay
Trade Name MACKAM®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay MACKAM® 2CSF-40CG Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Mackam 2CSF-40CG is an alcohol and salt free, mild, amphoteric surfactant with applications in both personal care and industrial formulations. In personal care products, Mackam 2CSF-40CG is used to couple conditioning agents into shampoos and body washes. This high foaming surfactant makes it an ideal choice when formulating mild shampoos, baby shampoos, or body washes. Mackam 2CSF-40CG is also useful in industrial cleaners due to its ability to couple nonionic surfactants into high levels of electrolytes and its broad pH range stability. Mackam 2CSF-40CG is an ideal choice for systems where sodium chloride would be detrimental to the performance of the final product or would cause corrosion problems. It also has the potential to reduce overall irritation of other surfactants. INCI NAME: Disodium Cocoamphodipropionate CAS: 68604-71-7 EINECS: 271-704-5: Uses: Baby Shampoos, Neutralizing shampoos, Body Wash, Alkaline built cleansers, and all purpose cleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Solids Content 38 - 40 %
38 - 40 %
Moisture Balance
pH 9.0 - 10
9.0 - 10
Viscosity <= 500 cP
<= 500 cP
#3 SP. @12 rpm
Optical Properties Metric English Comments
Gardner Color Number <= 7.0
<= 7.0
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Alcohol
&lt;0.1%
Gram Negative Bacteria
Absent
Total Plate Count
&lt;10 cfu/g