Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 350 - 450 cP @Temperature 23.0 °C |
350 - 450 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Viscosity | 350 - 650 cP | 350 - 650 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 45-40/05 Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: DIY, AutomotiveInformation provided by Merquinsa |
|||
Viscosity | 350 - 450 cP | 350 - 450 cP | |
Huntsman CY 179 MA Multifunctional Resin Weight per Epoxide (EEW, g/eq) 131 to 143. Max color is 1.Comments/Applications: Alicyclic diepoxy carboxylate, low viscosity liquid epoxy. High temperature outdoor electrical and casting applicat.. |
|||
Viscosity | 350 - 450 cP | 350 - 450 cP | |
Lord Adhesives Metech 2232 Silver Conductor This product is a silver bearing, thermoplastic, acrylic, polymer paint designed primarily as a conductive electrode solder base for tantalum capacitors. Additionally, this material can be used as a.. |
|||
Viscosity | 350 - 590 cP | 350 - 590 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1117 P (SIS) Linear Triblock Copolymer Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | 350 - 490 cP | 350 - 490 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1133 K (SBS) Linear Triblock Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 350 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | RPG30 |
Solvay ALKAMULS® EL 620 LI E Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€.. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | #3 SP @ 60 RPM; RP-0659 |
Solvay ALKAMULS® EL 620LI Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5A.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8026 Silicone Stabilizer for PU Foam STRUKSILON 8026 is used as a silicone stabilizer for the production of polyurethane shoe sole systems as well as other microcellular foams. It is especially recommended for shoe sole formulations ba.. |
|||
Viscosity | <= 350 cP @Temperature 25.0 °C |
<= 350 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E5 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3210 Polyester, Pellet Medium Tg, standard resin, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
Mixed (sp #2, 10 rpm) |
Tra-Con Tra-Bond FS437 Low Viscosity High Impact Epoxy Adhesive TRA-BOND FS437 is a two-part, low viscosity material formulated for optical applications which require excellent wicking, visible color and high strength. This material has been used successfully fo.. |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7600 Coating Syl-off® 7600 coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer.Information provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 200 Coating Low release at high speeds; high viscosityInformation provided by Dow Corning |
|||
Viscosity | 350 cP | 350 cP | dynamic |
Dow Corning SYL-OFF® SL 200 COATING Low release at high speeds; high viscosityInformation provided by Dow Corning |
|||
Viscosity | 350 - 650 cP @Temperature 23.0 °C |
350 - 650 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Viscosity | 350 - 550 cP @Temperature 23.0 °C |
350 - 550 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |
|||
Viscosity | 350 cP | 350 cP | B Component; Spindle #2; speed 50 rpm; ASTM D1824 |
Aptek 6100-1A/B Epoxy Encapsulant Optoelectronic grade, water clear encapsulant for IR and visible LED discreet devices. Lower Tg versions available for display devices.Part A is dark blue. Part B is clear to pale yellow.Information.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 350 cP @Temperature 200 °C |
350 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3600 Polyester, Pellet High Tg, PET adhesiveness, Transparency, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, .. |
|||
Viscosity | 350 cP @Temperature 40.0 °C |
350 cP @Temperature 104 °F |
Solution, 25% in Dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | Part B |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |