Kraton® D1117 P (SIS) Linear Triblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1117 P (SIS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: Kraton D1117 PT - supplied as a dusted dense pelletRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1117 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Viscosity 350 - 590 cP
350 - 590 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.30 - 0.40 %
0.30 - 0.40 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 33

@Time 10.0 sec
33

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 8.27 MPa
1200 psi
Typical properties on film cast from toluene solution; ASTM D412
Elongation at Break 1300 %
1300 %
Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.000414 GPa
0.0600 ksi
Typical properties of film cast form toluene solution; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 33 %
33 %
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.3%, KM 08
Polystyrene
15.6-19.2%, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 17/83